ICP Spectroscopy
In ICP Spectroscopy samples are acid digested and diluted in water and aspirated into a plasma torch. The emitted light is then measured and quantified relative to known standards. ICP is a very versatile spectroscopic technique, capable of analyzing a full spectrum of samples from water samples to dissolved alloys of Steel, Aluminum, Brass, Titanium and Nickel based alloys. ICP Spectroscopy is used to accurately determine the chemical composition of ferrous and nonferrous alloys as well as a variety of other samples and extracts. Our lab currently uses a SpectroFlame M120E spectrometer. The standards used for analyses are traceable to NIST.
NHML Brochure
- October 4, 2010 - Our Latest Brochure
Latest Resources
- October 10, 2011 - Periodic Table of Elements
- February 7, 2011 - Alloying Elements Table
- September 15, 2010 - Aluminum Anodizing Defects
- January 31, 2010 - Corrosion Of Aluminum Hardware – Case History of Corrosion Of Aluminum Hardware
- June 25, 2009 - Case History: Wind Turbine Manufacturer –
Case history from Metallurgical Department of NHML.
Latest Newsletters
- October 14, 2011 - Nuts & Bolts - Supplemental Edition Issue 6 - Decontamination
- October 7, 2011 - Special Bulletin: Decontaminating Biomedical and Pharmaceutical Products –
NHML guest author describes in detail the detail involving the decontaminating of biomedical and pharmaceutical products.
- September 1, 2011 - Nuts & Bolts - Supplemental Edition – Polymers and the Medical Device Industry
- May 1, 2011 - Nuts & Bolts Supplemental Issue - Benefits of Load Testing Analysis – Benefits of Load Testing Analysis